ʻO Resin-SZUV-S9006-kiʻekiʻe kiʻekiʻe
Hoʻolauna i nā mea paʻi 3D
Nā hiʻohiʻona
SZUV-S9006
HOIKE HUA
ʻO SZUV-S9006 kahi ABS e like me SL resin i loaʻaʻoʻoleʻa kiʻekiʻehiʻona. Hoʻolālā ʻia ia no nā paʻi paʻi SLA mokuʻāina paʻa. Hiki ke hoʻohana ʻia ʻo SZUV-S9006 i nā kumu kumu, nā kumu hoʻohālike, nā ʻāpana hui a me nā prototypes hana ma ke kahua o nā ʻoihana kaʻa, nā lāʻau lapaʻau a me nā mea kūʻai aku. ʻO ke kūkulu ʻana o nā ʻāpana me SZUV-S9006 ma luna o 6.5 mau mahina.
ANOAIHIʻona
- ʻO ka viscosity liʻiliʻi o ka resin wai, no laila maʻalahi ka hoʻihoʻi hou ʻana, maʻalahi e hoʻomaʻemaʻe i nā ʻāpana a me nā mīkini
- Hoʻonui i ka ikaika i hoʻopaʻa ʻia, hoʻomaikaʻi ʻia ka nui o ka mālama ʻana o nā ʻāpana i kahi kūlana haʻahaʻa
- pono ka hoʻopau hapa liʻiliʻi
-Loaʻa ke ola o ka mīkini
-Haʻahaʻaʻokiʻoki lalo
ANOAIPOMAIKAI
- Pono ka liʻiliʻi o ka manawa hoʻopau ʻana, maʻalahi ma hope o ka hoʻōla ʻana
- Bulid pololei a me nā ʻāpana paʻakikī kiʻekiʻe me kahi kūpaʻa dimensional i hoʻomaikaʻi ʻia
- Nā mana kiʻekiʻe no ka hoʻolei ʻana i nā ʻāpana
-ʻO ka emi haʻahaʻa a me ke kū'ē maikaʻi i ka melemele
-ʻO ke kala keʻokeʻo nani
- ʻO nā mea SLA machinable maikaʻi loa
Hoʻomaopopo: ʻaʻole pono ke kiʻekiʻe loa ka mahana o szuv-s9006. E ʻoluʻolu e hoʻohana iā ia ma lalo o 25 ℃. Pono ka haʻahaʻa haʻahaʻa no ka hoʻohana ʻana a me ka mālama ʻana ma lalo o 38RH%.
KEKAHI O KA'U HANA
Hoʻonaʻauao
Nā Molu lima
Nā ʻāpana kaʻa
Hoʻolālā Packaging
Hoʻolālā Kiʻi
Lapaau
Nā Waiwai Kino (Liquid)
Ka nana aku | Keʻokeʻo |
ʻO ka mānoanoa | 1.11-~1.15g/cm3@ 25 ℃ |
Viscosity | 230~290cps @ 26 ℃ |
Dp | 0.13~0.145 mm |
Ec | 9.5~10.5 mJ/cm2 |
Mānoanoa papa hale | 0.05~0.12mm |
Mea Mechanical (Post-Cured)
ANA | ANOAI HOAO | WAIWAI |
90 mau minuke UV ma hope o ka ho'ōla | ||
Paʻakiki, Kahakai D | ASTM D 2240 | 75-85 |
Hoʻololi hoʻololi, Mpa | ASTM D 790 | 2,592-2,675 |
Ka ikaika wiliwili, Mpa | ASTM D 790 | 63-70 |
ʻO ka modulus tensile, MPa | ASTM D 638 | 2,489-2,595 |
Ka ikaika uʻi, MPa | ASTM D 638 | 36-53 |
ʻO ka hoʻolōʻihi i ka wā hoʻomaha | ASTM D 638 | 15-25% |
Ka ratio o Poisson | ASTM D 638 | 0.4-0.44 |
ʻIke ʻia ka ikaika o ka hopena Izod, J/m | ASTM D 256 | 45-70 |
ʻO ka wela wela, ℃ | ASTM D 648 @66PSI | 38-50 |
Hoololi aniani,Tg | DMA,E”peak | 40-54 |
Coefficient o ka lilo wela | TMA(T | 90~102*E-6 |
Māmā, g/cm3 | 1.12-1.18 | |
Dielectric Constant60 Hz | ASTM D 150-98 | 4.2-5.0 |
Dielectric mau 1 kHz | ASTM D 150-98 | 3.3-4.2 |
Dielectric Constant1 MHz | ASTM D 150-98 | 3.2-4.0 |
Ka ikaika dielectrickV/mm | ASTM D 1549-97a | 12.8-16.1 |